Abstract
The authors measured the profile of second harmonics during B-H hysteresis loop as a function of the tensile stress and the angle φ, between the H-field applied and the [100] axis in (110)[001] grain oriented 3% silicon iron. The variation of anisotrophy field is discussed in terms of the domain reorientation under the field and tensile stress. This analysis provides the basis for easy access of anisotropy field, compared to the conventional technique.
| Original language | English |
|---|---|
| Pages (from-to) | BS-09 |
| Journal | Digests of the Intermag Conference |
| State | Published - 2000 |
| Event | 2000 IEEE International Magnetics Conference-2000 IEEE INTERMAG - Toronto, Ont, Can Duration: 9 Apr 2000 → 13 Apr 2000 |