Deformation behavior during nanoindentation of epitaxial ZnO thin films on sapphire substrate

R. Navamathavan, Kyoung Kook Kim, Dae Kue Hwang, Seong Ju Park, Tae Geol Lee, Gwang Seok Kim, Jun Hee Hahn

Research output: Contribution to journalArticlepeer-review

7 Scopus citations

Fingerprint

Dive into the research topics of 'Deformation behavior during nanoindentation of epitaxial ZnO thin films on sapphire substrate'. Together they form a unique fingerprint.

Material Science

Engineering